Good Afternoon,

I am appending the following for a fellow engineer in my dept. that
does not have the capability to append directly. I will forward any
and all responses to Mr. Ayotte - Thx. In Advance...Jay Edwards
-------------
  With respect to the attached ATT response; what I am wondering is:

   - what are the voltage applications for the products that ATT
      uses single sheet prepregs in?
   - is this true for signal/signal, signal/power and power/power
      applications?
   - what are the reliability requirements for the products this
      is being used in (0.1 ppm/KPOH or 10 ppm/KPOH or higher)?
   - is this consumer products, games and toys or mainframe?
   - what prepreg thickness/thinness does ATT use?

   Any and all information is greatly appreciated.  Thanks in
      advance           Stephen Ayotte, IBM MD Quality Engineer
************************************************************************
  Received: from gagme.wwa.com by vnet.IBM.COM (IBM VM SMTP V2R3) with TCP;
     Wed, 24 May 95 13:11:24 EDT
  Received: from ipc by gagme.wwa.com with uucp
  º(Smail3.1.28.1 #8) id m0sEJSm-000FHYC; Wed, 24 May 95 11:39 CDT
  Received: by ipchq.com (Smail3.1.28.1 #2)
  ºid m0sEItM-0000GmC; Wed, 24 May 95 11:02 CDT
  Old-Return-Path: <miso!attme.att.com!rgrrh>
  Message-Id: <[log in to unmask]>
  Date: 24 May 95 10:18:06 -0400
  To: [log in to unmask], [log in to unmask]
  From: [log in to unmask] (R_R_HOLMES)
  Original-Date: Wed May 24 10:18:06 EDT 1995
  Phone: (804) 226-5114
  Subject: Re: single ply dielectric and "green" laminate
  Original-To: compuserve.com!100430.2627
  Original-To: [log in to unmask]
  In-Reply-To: your message  of May 22 18:28:11 EDT 95
  Content-Type: Text
  Resent-Message-ID: <"6GyxY3.0.wvD.VYrml"@ipc>
  Resent-From: [log in to unmask]
  X-Mailing-List: <[log in to unmask]> archive/latest/535
  X-Loop: [log in to unmask]
  Precedence: list
  Resent-Sender: [log in to unmask]

  AT&T has been using single ply B-stage for several years and is in the process
  of converting all product to single sheet.  We have seen no reliability
  problems, and believe that a single ply is as reliable as two plies. We are in
  the process of converting all products to single sheet (5 mil, 6 mil, 8 mil 10
  mil).  We also make PCMCIA cards with 2.8 mil single sheet glass.

  The only real risk with single sheet glass is the possibility that a
  dielectric void could bridge layer to layer through the glass cloth.  With
  modern PWB processes this is a limited risk. In addition, in some cases, a
  tight weave single sheet glass provides a tighter barrier than two sheets of
  an open weave.  The only field problem that I remember actually occured with
  two sheets of an open weave (1080 glass).

  In conclusion, AT&T believes that single sheet constructions are very reliable
  and we are using them in most of our products.
  º------------- Begin Original Message -------------
  Message-Version: 2
  From: compuserve.com!100430.2627
  Date: May 22 18:28:11 EDT 95
  Received: from attme by attme.cnet.att.com; Tue, 23 May 1995 12:03 EDT
  Received: from att!wwa.com!ipc!ipchq.com by ig2.att.att.com id AA23053; Tue,
  23 May 95 11:07:54 EDT
  Received: by gw2.att.com; Tue May 23 11:08:31 EST 1995
  Received: from ipc by gagme.wwa.com with uucp
  Received: (Smail3.1.28.1 #8) id m0sDvZG-000FHuC; Tue, 23 May 95 10:08 CDT
  Received: by ipchq.com (Smail3.1.28.1 #2)
  Received: id m0sDuxN-0000GqC; Tue, 23 May 95 09:29 CDT
  End-of-Header:
  Email-Version: 2
  Subject: single ply dielectric and "green" laminate
  Resent-Date: 22 May 95 18:28:11 EDT
  Old-Return-Path: <miso!compuserve.com!100430.2627>
  To: [log in to unmask]
  Message-ID: <[log in to unmask]>
  Resent-Message-Id: <"uIUpG3.0.d59.p4Vml"@ipc>
  Resent-From: [log in to unmask]
  X-Mailing-List: <[log in to unmask]> archive/latest/533
  X-Loop: [log in to unmask]
  Precedence: list
  Resent-Sender: [log in to unmask]
  End-of-Protocol:
  Content-Type: text
  Content-Length: 545

  To what extent has the PCB industry changed to single ply for pre-preg as
  opposed to core which has been available in single ply for a long time.  What
  are the fears about single ply pre-preg? Are 2 plies really better than 1
  thickone?

  What are the attitudes towards so called "green laminate"? Is it simply a case
  of eliminating bromine, is it vital to meet UL V- 0 if the alternative could
  have such an impact on the environment?

  These questions were prompted by a major user of PCBs in Europe.

  George Wheadon  Nelco UK