In a message dated 5/21/03 5:03:38 PM Central Daylight Time,
[log in to unmask] writes:
Phil,
I believe what the question refers to is the nickel/tin alloy which some
people call the Santaclara process. This was developed several years ago for the
telecommunications industry to minimize corrosion. However, it is not a very
reliable surface to solder to and was abandoned by most users.
Larry
> hi,
>
> I think, but am not certain, that I understand your question.
>
> First of all, I interpret nickel/tin plating to be 'pure' nickel with 'pure'
> tin deposited on top of it. If this is the case, you haven't gotten rid of
> the magnetic nickel.
>
> second, nickel-only is not a good finish to solder to say the least
>
> third, specifically, what do you mean by reliability?
>
> Phil
>
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|