Sender: |
|
X-To: |
|
Date: |
Fri, 25 Jul 2008 19:12:00 +0300 |
Reply-To: |
|
Subject: |
|
From: |
|
Content-Transfer-Encoding: |
quoted-printable |
In-Reply-To: |
|
Content-Type: |
text/plain; charset=ISO-8859-15; format=flowed |
MIME-Version: |
1.0 |
Parts/Attachments: |
|
|
1. with a good water wash, just th same as when you solder the beastie
with a WS flux. No messing, no short cuts.
2. categorically NO! Alcohol may not dissolve the residues, either
organic or metallic
3. Yes! This is why you need to give it a full-scale wash. You cannot
clean with a brush: all you will do is harm by spreading those ionics
all over the place.
WS=WATER soluble - un point, c'est tout!
Brian
Jean-François Bissonnette wrote:
> Hello Technetters,
>
>
>
> We experienced some problems after reworking circuit boards, I would like to have inputs on the following.
>
>
>
> The problem found is capacitor leakage. The capacitor was added manually after automated production. The boards were coated with acrylic conformal coating.
>
>
>
> 1- How should a WS flux be cleaned after a rework?
>
> 2- Can WS be cleaned with alcohol? If not what would happen?
>
> 3- When reworking a SMT component, can WS flux be trapped under the component and cause leakage. The rework was cleaned with a brush or similar method.
>
>
>
> We think that the rework method was as follow (to fix a possible contamination under the component)
>
> a- SMT component is removed (possibly directly through the conformal coating)
>
> b- Using coating thinner, the area is cleaned and verified under UV to ensure no coating is present.
>
> c- WS flux is added
>
> d- Component is soldered back in place
>
> e- Area is cleaned with isopropyl alcohol
>
> f- Coating is added
>
>
>
> I think I've read that cleaning WS flux with alcohol is a NO NO! Can anyone confirm and comment?
>
>
>
> Jean-Francois
>
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|