TECHNET Archives

July 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Jean-François Bissonnette <[log in to unmask]>
Date:
Fri, 25 Jul 2008 19:12:00 +0300
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
From:
Brian Ellis <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset=ISO-8859-15; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (81 lines)
1. with a good water wash, just th same as when you solder the beastie 
with a WS flux. No messing, no short cuts.

2. categorically NO! Alcohol may not dissolve the residues, either 
organic or metallic

3. Yes! This is why you need to give it a full-scale wash. You cannot 
clean with a brush: all you will do is harm by spreading those ionics 
all over the place.

WS=WATER soluble - un point, c'est tout!

Brian

Jean-François Bissonnette wrote:
> Hello Technetters,
> 
>  
> 
> We experienced some problems after reworking circuit boards, I would like to have inputs on the following.
> 
>  
> 
> The problem found is capacitor leakage.  The capacitor was added manually after automated production.  The boards were coated with acrylic conformal coating.
> 
>  
> 
> 1-       How should a WS flux be cleaned after a rework?
> 
> 2-       Can WS be cleaned with alcohol?  If not what would happen?
> 
> 3-       When reworking a SMT component, can WS flux be trapped under the component and cause leakage.  The rework was cleaned with a brush or similar method.
> 
>  
> 
> We think that the rework method was as follow (to fix a possible contamination under the component)
> 
> a-       SMT component is removed (possibly directly through the conformal coating)
> 
> b-       Using coating thinner, the area is cleaned and verified under UV to ensure no coating is present.
> 
> c-       WS flux is added
> 
> d-       Component is soldered back in place
> 
> e-       Area is cleaned with isopropyl alcohol
> 
> f-         Coating is added
> 
>  
> 
> I think I've read that cleaning WS flux with alcohol is a NO NO!  Can anyone confirm and comment? 
> 
>  
> 
> Jean-Francois 
> 
>  
> 
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2