Please be cautious, different boards have different profiles, I agree that
the temperature and time indicated below are good starting values.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Blanchet,Richard
Sent: Monday, December 22, 1997 2:01 PM
To: [log in to unmask]
Subject: [TN] FW: [TN] Wave solder temp


250 - 260 oC

2 - 5 seconds.

 ----------
From: owner-technet
To: TechNet
Subject: [TN] Wave solder temp