Please be cautious, different boards have different profiles, I agree that the temperature and time indicated below are good starting values. -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Blanchet,Richard Sent: Monday, December 22, 1997 2:01 PM To: [log in to unmask] Subject: [TN] FW: [TN] Wave solder temp 250 - 260 oC 2 - 5 seconds. ---------- From: owner-technet To: TechNet Subject: [TN] Wave solder temp