TECHNET Archives

March 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Somtawin Pornpottanamas <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Tue, 16 Mar 2004 23:44:00 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (34 lines)
Now we have some problem in one component. The component was plated
Nickel (electroplated) , and  base material is phosphor bronze. The
problem we found was solderability failed. We try to find out what's the
cause. We have to inspect the solderability   by dipping test before
passed to the line. Some failed some passed. we had done the analysis to
compare the good one and bad one. We had check Nickel thickness (XRF,
cross section), phosphorus content and grain structure (by SEM & EDX).
From  the data , it show the different. But we don't know how does it
effect to the solderability. Does anyone know what 's the parameter that
affect to solderability, how? And what 's about the contaminate in
Nickel bath ? 

From EDX we found Fe element in bad part, does Fe effect to
solderability? 

 

Thanks & Regards,

Somtawin Pornpottanamas

 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2