TECHNET Archives

March 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0w7tIA-000BBjC; Thu, 20 Mar 97 19:38 CST
From [log in to unmask] Fri Mar 21 11:
17:56 1997
Date:
Thu, 20 Mar 1997 20:48:33 -0500 (EST)
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/11257
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"3dTuy1.0.caJ.fQUCp"@ipc>
Subject:
From:
Old-Return-Path:
X-Loop:
Message-ID:
Parts/Attachments:
text/plain (20 lines)
It is very important to know the cure conditions of both coatings,
application procedure and thickness. One situation you want to avoid is
overcuring the solder mask prior to conformal coating application.  It is
true if you apply a thicker coating you may solve the problem, but that is
neither the right approach or the best approach.  Your system could be clean
but totally overcured where anything you apply may have adhesion problems.  
There are other possibilities, but first provide the information above.

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2