On controlling the amount of flux:
* A paint brush scheme or a little dab'ldoya are a bit too flakey
* BIG timers have these fancy flux depth controller machines that squirt
flux onto a plate. It has a wiper that goes around in circles [driven by a
motor under the plate and its shaft poking perpendicularly through the
plate ]. But then again, this is a production process thing, not a rework
thing.
* We use a credit card with a portion of the edge cut away to leave a tooth
on each end. We drag it through the paste to level it out, before dipping
the component.
Dave Fish
----- Original Message -----
From: "PHC L.L." <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, February 04, 2002 10:24 AM
Subject: Re: [TN] BGA Rework Using Paste vs. No Paste
> By the way... How much flux do you apply for this
> no-paste BGA rework? How do you control the volume of
> the flux? Any particular tools?
>
> Thanks
>
>
>
>
> >It's a matter of useful information, not raw
> data(BS). I'll show you mine
> if you'll show me yours.
>
> Seems like most folks have shown their all and it
> appears in favor of less
> is more but as Daan said, more only is 10%. What's
> IPC's take on all this.
> What standard/rule/data/info is right. Most all of
> industry, as exemplified
> on this forum, points to paste flux, for rework
> instead of solder paste,
> whether applied crudely, rudely, or with MoonMan's
> flare for exactomundo by
> microstenciling the stuff.
>
> The MoonMan's and Werner's take to all this is flux
> it. It's still too
> simple to flux up but where are the standards?
>
> Thanks Dave for putting it all into perspective, or
> not.
>
> MoonMan
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC
> using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask]
> with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send
> e-mail to [log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line
> Resources & Databases > E-mail Archives
> Please visit IPC web site
> (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at
> [log in to unmask] or 847-509-9700 ext.5315
> --------------------------------------------------------------------------
-------
>
>
> __________________________________________________
> Do You Yahoo!?
> Great stuff seeking new owners in Yahoo! Auctions!
> http://auctions.yahoo.com
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|