TECHNET Archives

July 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset=us-ascii
Sender:
Subject:
From:
"<Peter George Duncan>" <[log in to unmask]>
Date:
Thu, 12 Jul 2001 08:29:30 +0800
MIME-Version:
1.0
X-To:
"COWEN,MARC (A-Scotland,ex1)" <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (104 lines)
Marc,

We can't, of course, see your sketch, but because you're having the
supplier specially form the legs, I imagine you've formed them into a gull
wing type configuration and kept the caps as surface mount (albeit a large
one).

For bonding, I recommend Eccobond 45. In my former life, we used it widely
on vulnerable components in the Eurofighter radar. It's an epoxy, rather
than an RTV, as I'm reluctant to use RTV on boards anyway.

Hope this helps a bit.

Pete Duncan




                    "COWEN,MARC
                    (A-Scotland,ex        To:     [log in to unmask]
                    1)"                   cc:     (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
                    <marc_cowen@AG        Subject:     [TN] PTH soldered onto smt pad
                    ILENT.COM>
                    Sent by:
                    TechNet
                    <[log in to unmask]
                    RG>


                    07/11/01 06:13
                    PM
                    Please respond
                    to "TechNet
                    E-Mail
                    Forum.";
                    Please respond
                    to "COWEN,MARC
                    (A-Scotland,ex
                    1)"






Hi All,

We currently have a modification to a PCA where we have added a capacitor.
Unfortunately the only capacitor suitable for this is a through hole
device.
We have therefore asked our supplier to form the legs as follows:











We have had instances where the solder on the left hand leg has not been
sufficient, the leg has come loose and this has worked like a spring. Also
the RTV compound we have also found to be unreliable.

Could some-one please advise of the following:

1.      Is there a better adhesive to use instead of RTV compound?
2.      Is there a quick and easy way for an inspector to check the solder
joint without placing undue stress on the capacitor legs or the solder
joint? We currently asking inspectors to "gently" try to move the leg while
looking at the solder fillet through a microscope to see if there is a
fracture.

Thanks for your help.

Marc.

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2