TECHNET Archives

April 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Marsico, James" <[log in to unmask]>
Date:
Wed, 11 Apr 2007 11:32:27 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Kevin Glidden <[log in to unmask]>
Subject:
From:
Kevin Glidden <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (138 lines)
I believe the intent is not to have the water draining from the surface for
a minute, rather that the water stays in the thin film (placed horizontally)
for 1 minute after the removal from the tank.  If the water beads up (like
on a waxed car) that indicates the contamination.  This test is often called
out for use on PCB surfaces prior to coating or even prior to bonding, but
in a modified manner in that you can simply squirt a little DI water from a
pipet onto the surface and see what happens - no dipping required.

Hope that helps,
Kevin


-----Original Message-----
From: Marsico, James [mailto:[log in to unmask]] 
Sent: Wednesday, April 11, 2007 10:28 AM
To: [log in to unmask]
Subject: Re: [TN] Water-break Test

I've been looking at ASTM F22-02, Standard test method for Hydrophobic
Surface Films by Water-Break Test.  The procedure is stated as follows:
"Withdraw the test surface, in a vertical position, from the container
overflowing with water."

The interpretation of results states:
"Surfaces tested ... shall be considered free of hydrophobic contaminants by
this test method if the draining water layer remains as a thin continuous
film over the surface for 1 min after withdrawal of the surface from the
overflow container.  If hydrophobic contaminants are present, as evidenced
by a formation of a discontinuous water film within 1 min after withdrawal
of the surface from the overflow container, the length of time necessary for
the water-break to occur is a rough indication of the degree of
contamination". 

Now, a couple of questions.  How can you expect all surfaces, assuming that
they are contamination free, to remain wet and draining for 1 minute after
removal from a tank?  Should this be 1 minute of continuous rinse?  What if
all of the water drains off before the minute is up, is that a failure?  In
my case, when removed from the water bath, the water remains a continuous
film for 15 seconds, after that, no more water remains.

Comments?

Jim Marsico
EDO Corporation
1250 New Horizons Blvd.
North Amityville, NY 11701
631-630-5079
[log in to unmask]
 
-----Original Message-----
From: Brian Ellis [mailto:[log in to unmask]]
Sent: Tuesday, April 10, 2007 2:40 AM
To: TechNet E-Mail Forum; Marsico, James
Subject: Re: [TN] Water-break Test

Before even trying to rely on the water break test, I suggest you may care
to read the peer-reviewed paper I presented in Circuit World, Volume 35,
Number 4, 2005. pp 47-50, entitled "The Water Break Test". 
This will explain that there are a number of fallacies involved, when
relying on such empirical methods. The main one is that the test will
succeed only on contaminated surfaces.

Brian

Marsico, James wrote:
> Hello Technet:
> 
>  
> 
> We have an application where we have to etch a PTFE PWB in preparation
> for bonding.   The etch is a commercially available sodium-containing
> solution.  We're also expected to meet a water-break test prior to 
> bonding.  We're having trouble meeting the water-break test and was 
> wondering if the two (etched PWB and water-break) are compatible.  If 
> so, what cleaning/rinsing could be performed after the etching to
ensure
> a water-break free surface?
> 
>  
> 
> Thanks in advance,
> 
>  
> 
> Jim Marsico
> 
> EDO Corporation
> 
> Amityville:  631-630-5079
> 
> Bohemia:  631-218-7057
> 
> [log in to unmask]
> 
>  
> 
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
> unsubscribe, send a message to [log in to unmask] with following text
in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt 
> or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
> -----------------------------------------------------
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2