Since anodizing is carried out by growing an oxide layer on the surface,
solderability of an anodizes stainless steel will be non-existent. Don't
forget that naturally stainless grows a thin chrome oxide layer which is
in the main what imparts its inherent corrosion resistance, so to solder
to it you need an extremely acid flux. The only stainless "anodizing"
treatment I know of is the Prismatic process (if aged brain remembers
correctly) and it is used to decoratively colour the surface by
thickening the oxide layer, different thickness gives different colour.
End result is not solderable unless you abrade the layer off and use a
highly acid flux
Regards
Ian Fox
Lead Materials and Process engineer
Goodrich ECS
York Road
Hall Green
Birmingham B28 8LN
United Kingdom
Tel: +44 (0)121 607 3763
Fax: +44 (0)121 607 3658
E-mail: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: 24 July 2008 16:38
To: [log in to unmask]
Subject: [TN] Anodizing Surface
Fellow TechNetters:
Is a Stainless Steel anodized surface solderable?
Victor,
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|