TECHNET Archives

September 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Paul Stolar <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 24 Sep 1998 08:35:17 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (68 lines)
Content-Transfer-Encoding: 7bit



     Under a hood of a car....hmmmmmm.

     There is a huge sulfer source there, the battery. Most batteries are
     still lead-sulfuric acid batteries.

     I suggest you look there.

     Now how do you prevent it. In a previous incarnation, we had to use
     parylene conformal coating.


______________________________ Reply Separator _________________________________
Subject: [TN] Open circuits from Silver Sulfide Corrosion
Author:  [log in to unmask]>                David Weber <[log in to unmask] at
internet
Date:    9/23/98 9:08 PM


I need help tracing the possible root causes for a circuit failure from
the field. Does anyone have any experience with open circuit traces due
to a silver sulfide corrosion concentrated at the juncture tin-lead
solder joints and silver thick films? We are seeing this only on joints
that are low voltage potential. There is silver sulfide corrosion at
other randomn areas, but the heavy corrosion is primarily at just a few
points where the solder and silver meet. Under the microscope, it looks
like a black worm crawling along the interface between the solder joint
& the silver thick film. We pot the circuit board in silicone gel to
protect the circuit from moisture. So far, we haven't traced the source
of sulfur to any material that we use to make or to package the circuit
board.
The packaging does not contain cardboard, so sulfur from the packaging
is out. We meticulously clean the board after reflow soldering the
printed solder paste, so flux is out. Is it possible that we are getting
sulfur gas from the enviroment? The environment is automotive,
underhood. Is it possible that there is a galvanic action that is
concentrating the corrosion to just a few solder joints?
Thank you all for your time.

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2