We have 2 selective soldering units supplied by an On-Site Gas N2 generator.
I calculate a purity >99.999% at the moment.
When we first started with N2, we used dewars supplied by a local gas
company. It wasn't long before we figured out it was more cost effective to
purchase our own generator.
Craig Sullivan
Manufacturing Engineer
MPL Incorporated
P: 607.266.0480 x115
F: 607.266.0482
[log in to unmask]
ƒÀ Please consider the environment before printing this e-mail.
Confidentiality Notice:
This e-mail contains privileged and confidential information which is the
property of MPL Incorporated, intended only for the use of the intended
recipient(s). Unauthorized use or disclosure of this information is
prohibited. If you are not an intended recipient, please immediately notify
MPL Incorporated and destroy any copies of this email. Receipt of this
e-mail shall not be deemed a waiver by MPL Incorporated of any privilege or
the confidential nature of the information.
Export Control:
This message is intended only for the addressee and may contain information
that is company confidential or privileged. Any technical data in this
message may be exported only in accordance with the U.S. International
Traffic in Arms Regulations (22 CFR Parts 120-130) or the Export
Administration Regulations (15 CFR Parts 730-774). Unauthorized use is
strictly prohibited and may be unlawful. If you are not the intended
recipient, or the person responsible for delivering to the intended
recipient, you should not read, copy, disclose or otherwise use this
message. If you have received this email in error, please delete it, and
advise the sender immediately.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Keith Calhoun
Sent: Tuesday, February 25, 2014 7:33 AM
To: [log in to unmask]
Subject: [TN] Nitrogen question
We are looking into installing a selective soldering machine in our
facility. The machine we are looking into wants a nitrogen supply to inert
the solder pot.
My question to the forum is what source are you using for their nitrogen
requirements? Also what purity level are you using?
Keith S. Calhoun
Manufacturing Engineering Manager
Sopark Corporation
3300 South Park Avenue
Lackawanna, New York 14218
716-822-0434 Ext. 237
[log in to unmask]
SoPark Corporation
Talent - Teamwork - Technology
Over 32 years as a Premier Electronics Manufacturing Service Provider ISO
9001:2008, ISO 13485:2003 & AS9100C Certified
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|