Kirk:

It has been some time since performing this test, but if memory serves
tin is measured chemically by ASTM E46; impurities (including copper,
gold, cadmium, zinc, aluminum, antimony, iron, arsenic, bismuth, silver,
and nickel), are measured spectrometrically (AA) by ASTM E663; and lead
is reported as the  "balance".

I am unsure of the ASTM designation for ICP determination, but the
general digestion method described in E663 may be the same for ICP.  If
silver is being determined, keep in mind aqua regia (HCl/HNO(3)) cannot
be employed as to dissolve the sample.

As previously mentioned, your current solder supplier should perform
this test for you AND provide you a copy of the method employed.

Regards,
Ted Stern

Kirk Kosel wrote:

>  Thanks for the responses.  One more question, any idea on how to get
> the solder (and impurities) in solution for ICP analysis? Thanks again
> for your help, Kirk

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2