TECHNET Archives

August 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Jan Satterfield <[log in to unmask]>
Date:
Wed, 12 Aug 1998 15:08:18 -0600
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (99 lines)
I think we need to clarify something here.  The original question was in
regards to a "dishwasher" type batch cleaner using a saponifier.  There
also exists  "semi-aqueous"  equipment that can be used with solvents
like Bioact EC-7 and IPA.  Under no circumstances should you attempt to
clean in a "dishwasher" type aqueous batch cleaner using solvents.
There could be a fire or explosion hazard.

>-----Original Message-----
>From:  Charles Barker [SMTP:[log in to unmask]]
>Sent:  Wednesday, August 12, 1998 2:52 PM
>To:    [log in to unmask]
>Subject:       Re: [TN] Batch cleaning of SMT RMA fluxes
>
>We used to batch clean RMA with one of the EC-7 family of solvents. I'm not
>sure what the rinse was made up of or if it was even anyhing other than DI
>water.
>
>We are now using Water Soluble for wave and reflow, RMA for hand soldering
>and cleaning all in an inline cleaner with Alpha 2110 and DI water. We did
>clean RMA from wave and reflow in this rig before going to WS.
>
>
>
>
>
>"Devitt, Kenneth" <[log in to unmask]> on 08/12/98 09:32:39 AM
>
>Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
>      to "Devitt, Kenneth" <[log in to unmask]>
>
>To:   [log in to unmask]
>cc:    (bcc: Charles Barker/US/I-O INC)
>Subject:  [TN] Batch cleaning of SMT RMA fluxes
>
>
>
>
>To TechNet,
>
>We are currently running a dishwasher type batch cleaner
>(AqueousTechnologies Model  RU400) and Kyzen XJN (30% concentration) are
>having difficulties removing flux residues from our SMT assemblies with RMA
>solder paste (ESP 63/37 RMA flux).
>
>Our current parameters are 155 F for wash chemistry for 9 Minutes,   100 F
>water rinse for total of 15 minutes, and 12 min. dry @ 120 F.
>
>We would like to hear from Techneters who are successfully using batch
>cleaners to remove RMA fluxes in terms of machine mfr., chemistry type,
>wash
>and rinse parameters.
>
>thanks in advance,
>
>Ken Devitt                              Tom Long
>[log in to unmask]        [log in to unmask]
>973-284-3880                    973-284-2786
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
>for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
>847-509-9700 ext.312
>################################################################
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
>for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
>847-509-9700 ext.312
>################################################################
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2