We are currently running a dishwasher type batch cleaner
(AqueousTechnologies Model RU400) and Kyzen XJN (30% concentration) are
having difficulties removing flux residues from our SMT assemblies with RMA
solder paste (ESP 63/37 RMA flux).
Our current parameters are 155 F for wash chemistry for 9 Minutes, 100 F
water rinse for total of 15 minutes, and 12 min. dry @ 120 F.
We would like to hear from Techneters who are successfully using batch
cleaners to remove RMA fluxes in terms of machine mfr., chemistry type, wash
and rinse parameters.
thanks in advance,
Ken Devitt Tom Long
[log in to unmask] [log in to unmask]
973-284-3880 973-284-2786
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|