      Hi Techneters


    During inner layer production the  AOI equipment  inspects and
determines which IL (inner layers ) should  be rejected. In the case that
there are several circuits in the inner layer panel , only the rejected
circuits should be marked before sending the inner layers to the following
processes.
We would like to find proper way to mark this rejected circuits in a way
that  we would be able to find them in the final electrical test .
For SPC purposes we would like to classify the boards  with opens & shorts
in stage of the final electrical test ,  which of them were rejected in the
previous AOI IL inspection . It means , that we have to know for sure ,
that specific circuit with opens or shorts was inspected , rejected & marked
during inner layer processes. 
Please, can anyone advice about proper method to mark the IL.
Edward Szpruch
Eltek Ltd - Israel
Tel  972 3 9395050
Fax 972 3 9309581
E-mail :  [log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2