TECHNET Archives

September 2017

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Frank Kimmey <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Frank Kimmey <[log in to unmask]>
Date:
Wed, 6 Sep 2017 17:14:00 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (1 lines)
Andy,

First question is What's a lot of RF power?

I've seen where 125+ watts can vaporize solderjoints, copper traces, vias, etc.

Even though you only measured 170C, I would not be surprised to find out the joint got much hotter very quickly and failed.

Any clue as to where the missing solder went to (I expect not)?

What size is the cap?

How wide is your trace in and out?

What is the finished copper weight?

Great pics by the way.

Good luck,

FNK



Frank N Kimmey CID+

Electrical Engineer / PCB Design

VeriFone Inc

1400 W Stanford Ranch Road, Suite 200

Rocklin, CA 95765 USA

W: 1-916-625-1818

M: 1-916-833-9877

[log in to unmask]



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Giamis, Andy

Sent: Wednesday, September 06, 2017 9:25 AM

To: [log in to unmask]

Subject: [TN] Crazy Solder



Hi TechNetters,



Here’s something I have not seen before.

I have seven different ‘theories’ for what’s happening here.

Three of which do not involve mythical creatures, illegal substances or the alignment of celestial bodies.



This capacitor is on a path that sees a lot of RF power.

The unit went through 20 cycles of -70C to +115C while at nominal power.  Temperature sensing suggests this device could be hitting 170C.

No, we normally don’t test to these extremes.

The PCB has ENiG finish and the solder is SAC.   This is normal SMT, no rework.



I think I know in general what happened, but I am surprised.

I don’t have an explanation for the formation of the big pocket on the right.

Has anyone ever come across any solder joints like this?



Thanks Steve for uploading the pictures (links below).



http://stevezeva.homestead.com/pockets_25.jpg



http://stevezeva.homestead.com/Pockets_CS.jpg



http://stevezeva.homestead.com/Pocket-left.jpg



http://stevezeva.homestead.com/Pockets-right.jpg





Best Regards,

Andy

Andrew C. Giamis

Senior Failure Analysis Engineer

CommScope

2601 Telecom Pkwy

Richardson, TX, 75082, USA





*********************************************************

This electronic message and any attachments are intended only for the use of the addressee. The information in this electronic message is confidential and proprietary, and may include privileged information. If you are not the intended recipient, please delete this electronic message and any attachments and notify the sender of the error. Please be aware that any unauthorized use, dissemination, distribution or copying of this message or any attachments is strictly prohibited.