Our pads were 0.2 mm but we did 1000's of them a day using a Type 4 lead
paste 100 micron stencil with very little problem once we got the
stencil sorted. DEK worked with us to do this all back in 2007!!! It was
considered difficult then! :-)
Regards
Rex
Rex Waygood
Technical Manager
Hansatech EMS provides value manufacturing through engineering and
quality
Hansatech EMS Limited
Benson Road
Nuffield Industrial Estate
Poole
Dorset BH17 0RY
United Kingdom
[log in to unmask]
www.HansatechEMS.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Amol Kane
(Asteelflash,US)
Sent: 16 August 2012 14:34
To: [log in to unmask]
Subject: [TN] CSP BGAs
Dear Technetters,
We are going to be assembling some lead-free 1.6x0.8 mm micro BGAs with
0.5mm pitch and 0.17mm dia board pads. Anybody else have experience with
this small a package?....I am concerned that there won't be sufficient
flux in the tiny solder deposit to clean the oxides during reflow,
leading to graping and/or head in pillow situation. Do I need a dip
fluxer for the part to do a flux only attachment, or to augment the
amount of flux in the solderpaste-solder bump system? I am told I have
no time to do DOEs to determine stencil and reflow parameters, so I am
turning to technet for help.....any thoughts?
Regards,
Amol
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the MessageLabs Email
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|