TECHNET Archives

September 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
R Sedlak <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, R Sedlak <[log in to unmask]>
Date:
Fri, 18 Sep 2009 08:34:50 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (216 lines)
It appears that Linda Langley's experience backs up your comment completely.
Rudy Sedlak
RD Chemical Company

--- On Fri, 9/18/09, [log in to unmask] <[log in to unmask]> wrote:

From: [log in to unmask] <[log in to unmask]>
Subject: Re: [TN] Black Pad
To: "TechNet E-Mail Forum" <[log in to unmask]>, "R Sedlak" <[log in to unmask]>
Cc: [log in to unmask]
Date: Friday, September 18, 2009, 6:53 AM



Hi Rudy - actually, if the copper and
tin form an intermetallic phase during your first pass thru the reflow
oven (which they should) then you would have solderability issues during
subsequent soldering operations.



Dave Hillman

Rockwell Collins

[log in to unmask]










R Sedlak <[log in to unmask]>


Sent by: TechNet <[log in to unmask]>
09/18/2009 08:44 AM



Please respond to

TechNet E-Mail Forum <[log in to unmask]>; Please respond to

R Sedlak <[log in to unmask]>






To
[log in to unmask]


cc




Subject
Re: [TN] Black Pad















Linda:

Actually, it is quite possible to get black immersion Tin.  
It comes from running a bath with an excess of Cupric Copper in it.  
I wrote a article on how to monitor Cupric Copper in immersion Tin baths
to avoid this in a recent PCD&F magazine.



The black color should not affect solderability, as it is actually immersion
Copper on top of the Tin.

Rudy Sedlak

RD Chemical Company



--- On Fri, 9/18/09, Linda Langley <[log in to unmask]> wrote:



From: Linda Langley <[log in to unmask]>

Subject: [TN] Black Pad

To: [log in to unmask]

Date: Friday, September 18, 2009, 3:12 AM



I know we have had this subject many times before so I did go to the

archives and still can't find an answer. My question, is Black Pad only

associated with ENIG? Is it possible with immersion Tin?



 



Linda Langley CIT



Training Specialist



Jabil Circuit



248-292-6176





---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text
in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]:
SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815

-----------------------------------------------------







      



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text
in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]:
SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815

-----------------------------------------------------






      

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2