Steve:
It ain't clear that the DI is doing it, but it does make sense, since the DI is SO much less conductive, lacking any ions in it, that it could hold a charge a lot better than tap water.
Maybe you want to consider using soft water, to eliminate the chlorides, but retain the ionic strength?
Rudy Sedlak
--- On Wed, 1/5/11, Steve Gregory <[log in to unmask]> wrote:
From: Steve Gregory <[log in to unmask]>
Subject: [TN] Deionized water in misting fans and static electricity
To: [log in to unmask]
Date: Wednesday, January 5, 2011, 10:31 AM
This may be an off the wall question but here goes.
We have some misting fans that we use for humidification that we've just
recently put in a deionized water source for.
Now it seems that there's a static charge being generated at the fans that
I've never noticed before. Could it be possible that we're generating a
charge at the fans because of the DI water?
Steve
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|