Does anyone have CTE, thermal conductivity, and strength data for
72Ag/28Cu brazing alloy? I'm performing a thermal/stress analysis of a
system that is cooling from solidification of the brazing alloy (800C)
to room temp. and is then modified and cooled to -55C. I'm sure the
properties are temperature dependent, but room temperature data would
get me in the ballpark. Any help would be appreciated.
______________________________________________________________________________
Bill Sturner - Structural/Thermal Analysis Voice: 609-338-2855
Lockheed Martin MARCALL: 8-794-2855
Government Communications Systems FAX: 609-338-2555,4628
1 Federal Street Email:
[log in to unmask]
MS: OPS-2-A1
Camden, New Jersey 08102
______________________________________________________________________________
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|