TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"David D. Hillman" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 29 Sep 2006 13:09:34 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (103 lines)
Hello Jose! Sorry but your question seems to be confused. If you are
looking for a solderability test that uses the wave solder machine then the
specification would be JSTD-002, if you are trying to determine how often
you should be testing the wave solder machine solderpot for element
contamination limits then the specification is JSTD-001. Hope this is
helpful.

Dave Hillman
Rockwell Collins
[log in to unmask]



             Jose Marroquin
             <jmarroquin@RAD-T
             ECH.NET>                                                   To
             Sent by: TechNet          [log in to unmask]
             <[log in to unmask]>                                          cc

                                                                   Subject
             09/29/2006 01:00          Re: [TN] Rocha Laminate Voids..
             PM


             Please respond to
              TechNet E-Mail
                   Forum
             <[log in to unmask]>
             ; Please respond
                    to
              Jose Marroquin
             <jmarroquin@RAD-T
                 ECH.NET>






Does anybody know the standard that calls for solderability test frequency
of the solder on the wave solder machine?


Jose R. Marroquin
Director of Quality Assurance
RAD Electronics, Inc.
(818) 381-8500
Fax (818) 381-8631


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Susan Mansilla
Sent: Wednesday, January 04, 2006 6:24 AM
To: [log in to unmask]
Subject: [TN] Rocha Laminate Voids..

Are there any vertical microsections of the laminate voids?  Have you
determined if they are in core laminate or in the prepreg laminate?  Do
they
appear
in the bare board prior to assembly?  Do they appear after assembly?

Susan Hott
Robisan Lab

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2