Hello Jose! Sorry but your question seems to be confused. If you are looking for a solderability test that uses the wave solder machine then the specification would be JSTD-002, if you are trying to determine how often you should be testing the wave solder machine solderpot for element contamination limits then the specification is JSTD-001. Hope this is helpful. Dave Hillman Rockwell Collins [log in to unmask] Jose Marroquin <jmarroquin@RAD-T ECH.NET> To Sent by: TechNet [log in to unmask] <[log in to unmask]> cc Subject 09/29/2006 01:00 Re: [TN] Rocha Laminate Voids.. PM Please respond to TechNet E-Mail Forum <[log in to unmask]> ; Please respond to Jose Marroquin <jmarroquin@RAD-T ECH.NET> Does anybody know the standard that calls for solderability test frequency of the solder on the wave solder machine? Jose R. Marroquin Director of Quality Assurance RAD Electronics, Inc. (818) 381-8500 Fax (818) 381-8631 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Susan Mansilla Sent: Wednesday, January 04, 2006 6:24 AM To: [log in to unmask] Subject: [TN] Rocha Laminate Voids.. Are there any vertical microsections of the laminate voids? Have you determined if they are in core laminate or in the prepreg laminate? Do they appear in the bare board prior to assembly? Do they appear after assembly? Susan Hott Robisan Lab --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------