TECHNET Archives

February 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 11 Feb 1998 20:09:34 -0600
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Keith Larson <[log in to unmask]>
Subject:
From:
Keith Larson <[log in to unmask]>
Content-Type:
multipart/mixed; boundary="------------28755308A3C56F831C61181E"
Organization:
Circuit Technology Inc.
MIME-Version:
1.0
Parts/Attachments:
text/plain (1303 bytes) , vcard.vcf (351 bytes)
Hi John,

Omikron is an immersion white tin finish offered by Florida CirTech in Greeley, CO. Try
1-800-686-6504.

Keith Larson
Circuit Technology Inc.

[log in to unmask] wrote:

>      Address,
>
>      I'm familiar with several surface finishes, but not Omikron (spelling
>      may be off).  Can someone shed some light on this surface finish.
>      I've run some testing for a customer and I am finding poor results.
>      The surface is very dull to begin with.  It almost looks like
>      Electroless SnNi or worse case Electroless SnPb.  Any how, insight
>      anyone.
>
>      Thanks,
>
>      John Gulley
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
> ################################################################




ATOM RSS1 RSS2