Hi John, Omikron is an immersion white tin finish offered by Florida CirTech in Greeley, CO. Try 1-800-686-6504. Keith Larson Circuit Technology Inc. [log in to unmask] wrote: > Address, > > I'm familiar with several surface finishes, but not Omikron (spelling > may be off). Can someone shed some light on this surface finish. > I've run some testing for a customer and I am finding poor results. > The surface is very dull to begin with. It almost looks like > Electroless SnNi or worse case Electroless SnPb. Any how, insight > anyone. > > Thanks, > > John Gulley > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. > For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 > ################################################################