TECHNET Archives

October 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 28 Oct 2008 12:31:12 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ted Tontis <[log in to unmask]>
Subject:
From:
Ted Tontis <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (181 lines)
Genny,

	Take a look at IPC-A-610C 1.3 specialized designs. 
In a nut shell it states 

1. The document can not cover all components. 
2. A decision/agreement needs to be made between the customer and the
supplier on acceptability of that component. 
3. If there are similar characteristics to a component already in the
document, you could use 610 as a guideline to start from.

I do not know what the end use application is but I would do some testing to
verify that solder on the component body would not have a negative impact on
the over all reliability of the component or solder joint. I work with
automotive lighting applications and we are constantly testing our
customer's new designs and processes for reliability due to the fact there
is little or no documentation on the assembly of new components/materials.
If there are issues or concerns prior to launch they are addressed with the
customer when exceptions can be made.

Regards,

Ted T. 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Green, Mike
Sent: Tuesday, October 28, 2008 11:53 AM
To: [log in to unmask]
Subject: Re: [TN] IPC-610, 8.2.5.5

I would think that you would have to take an exception on the drawing
until IPC -A-610 provides direction for each special case design.

Solder touching the component is a defect because most components are
not designed to withstand the stress internally of molten solder
temperatures.  
In addition, the solder joint in contact with a case puts the joint
subject to the CTE excursions of that case.  For example, as a plastic
case expands, it pushes against the solder joint causing thermal stress

Mike Green
Electronic Packaging Design
LMCO-Sunnyvale
408-743-1635
One Corporation, One Team

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Monday, October 27, 2008 10:13 AM
To: [log in to unmask]
Subject: Re: [TN] IPC-610, 8.2.5.5

Hi Genny!

Sorry it took me a bit to get your picture posted, but you know how
Monday mornings can be. I've got it up now though, it's at:

http://stevezeva.homestead.com/files/tsfp-3.GIF


Steve

-----Original Message-----
From: Genny Gibbard [mailto:[log in to unmask]] 
Sent: Monday, October 27, 2008 9:58 AM
To: TechNet E-Mail Forum; Gumpert, Ben
Cc: Steve Gregory
Subject: RE: [TN] IPC-610, 8.2.5.5

I don't know.  I've included a graphic.  Steve could you post it please?


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gumpert, Ben
Sent: October 27, 2008 5:10 AM
To: [log in to unmask]
Subject: Re: [TN] IPC-610, 8.2.5.5

Genny,

It sounds like you have something that has terminations similar to a
QFN/DFN but where the lead frame is not trimmed flush to the component
body. Is there exposed metal an the bottom side of the component, or are
the leads really coming out of the side of the component?

Are you sure that section 8.2.13 is not more applicable?

Ben

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Genny Gibbard
Sent: Friday, October 24, 2008 6:22 PM
To: [log in to unmask]
Subject: [TN] IPC-610, 8.2.5.5

Question for the TechNet gurus.
The spec in the subject says that solder touching the component body is
a defect.  But it states that it is allowed for SOTs.
We use a component in a TSFP (thin small flat package).  The
configuration like a 3 lead sot, but the leads are not gullwing - they
come straight out of the device and the whole package mounts flat onto
the board.  It is much smaller than a SOT, on the order of ~1.2mm sq in
total area.
Does this fit in the definition of a SOT?  
The recommended layout actually has the pads start under the device
body.  I'm not sure how you could possibly avoid solder touching the
body.

In general, why is it a defect for solder to touch the component body
for other component types?
Thanks so much for your help.

Genny 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2