TECHNET Archives

February 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
"Joseph E. J. Duclos Jr." <[log in to unmask]>
Date:
Wed, 4 Feb 1998 07:18:12 -0500
Content-Type:
multipart/mixed; boundary="---- =_NextPart_000_01BD313D.5F52F440"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Joseph E. J. Duclos Jr." <[log in to unmask]>
Parts/Attachments:
text/plain (1608 bytes) , application/ms-tnef (2881 bytes)
Ken, you should get 2 boards on a panel.

Run the 8.414" in the 21" dim - space boards by appx 1" or so to miss multi-line standard tooling locations for multilayer.
The 16.994 will fit snugly but shud be okay in the 18" - if you have enough pre-preg, you should have no problems.

JOE SENDZ.....


-----Original Message-----
From:   Ken Patel [SMTP:[log in to unmask]]
Sent:   Tuesday, February 03, 1998 9:29 PM
To:     [log in to unmask]
Subject:        [TN] panel yield on back plane

How many back plane boards I can expect from a panel of 18"X21" panel size.
The thickness of the board is 125 mils. My board size is 8.414" X 16.994".
Also if I get only one board then what dimension should I reduce to get 2
per panel.

re,
ken patel
______________________________________________________
Ken Patel                       Phone:  (408) 490-6804
1708 McCarthy Blvd.             Fax:    (408) 490-6859
Milpitas, CA 95035              Beeper: (888) 769-1808

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2