Yes the oxide reduction process works well. It also in improved upon if you
bake after drill.  To test this theory Just drill a few panels with a solid
oxide core. Bake half then etch off the outside copper,  You will see a
significant difference.

Another popular approach being used in double treated and resin coated foil
which does not require a black oxide.

Ed Cosper


-----Original Message-----
From: [log in to unmask] <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Thursday, May 06, 1999 1:24 PM
Subject: [TN] Black oxide process


>In producing multilayer PCB's, there is an oxide process used to prevent
pink
>ring.  Usually this process is called the "black oxide process" and
requires use
>of a reducer solution containing an amine borane.
>
>Is this process considered a standard in the PCB industry and is it's use
>increasing?
>
>Are there alternative processes which accomplish the same objective?
>
>What is the future trend to eliminate pink ring?
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2