TECHNET Archives

June 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Craig Hillman <[log in to unmask]>
Date:
Wed, 27 Jun 2001 16:45:15 +0100
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Peter Swanson <[log in to unmask]>
Subject:
From:
Peter Swanson <[log in to unmask]>
X-cc:
"Bob WILLIS (E-mail)" <[log in to unmask]>, "Tony GORDON (E-mail)" <[log in to unmask]>
Content-Type:
text/plain
MIME-Version:
1.0
Parts/Attachments:
text/plain (104 lines)
Craig,

The SMART Group ran a small survey on this recently -
http:www.smartgroup.org, click on surveys on the left menu bar, I think
it was Jan this year. It wasn't CEM-specific, nor very detailed. Maybe
future surveys will elaborate.

Regards,
Peter
--
=========================================================
Peter Swanson            [log in to unmask]
INTERTRONICS                http://www.intertronics.co.uk

INTERTRONICS is dedicated to providing quality material,
  consumable and equipment solutions to the electronics
manufacturing and other technology based industries, with
   the highest levels of technical support and customer
                         service.


-----Original Message-----
From: Craig Hillman [mailto:[log in to unmask]]
Sent: 27 June 2001 15:28
To: [log in to unmask]
Subject: [TN] How do you reflow?


Werner brings up an interesting point. Does anyone have an opinion on
the
trends in solder reflow in the contract assembly industry? Are we seeing
a
resurgence in vapor phase? Has flowing nitrogen during infrared fallen
to
the wayside? Interested in seeing your responses.

Best Regards,
Craig



-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Werner Engelmaier
Sent: Thursday, May 31, 2001 1:19 PM
To: [log in to unmask]
Subject: Re: [TN] AW: [TN] Pad in Via for BGA's - Part II


Hi Rush,
Vapor phase soldering was and is thew most elegant engineering solution
to
soldering--no over-temperatures, no profiles, absolute temperature
uniformity. What killed this approach in the past was inadequate
equipment--thhis is no loger a problem.

Werner Engelmaier

------------------------------------------------------------------------
----
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases
>
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
------------------------------------------------------------------------
----
-----

------------------------------------------------------------------------
---------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases
> E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
------------------------------------------------------------------------
---------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2