TECHNET Archives

June 2002

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Tempea, Ioan" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 20 Jun 2002 16:00:41 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (339 lines)
Thanks everybody for the input.

Now it's clear to me that mild flux no-clean waving after 2 reflows won't
exactly be successful with ImSn.

Regards,
Ioan

> -----Original Message-----
> From: Steve Kelly [SMTP:[log in to unmask]]
> Sent: Thursday, June 20, 2002 9:24 AM
> To:   [log in to unmask]
> Subject:      Re: [TN] Immersion Tin
>
> 1) we send samples to our chemistry supplier every 3 months to run the
> SERA
> 2) tight control of the chemistry on the line - actually not very
> difficult
> 3) after 5 years of running this I can look at the finish and tell with
> probably a 99.9% accuracy if it is acceptable
> 4) we also do solderability tests
> 5) 5 years of 0 field returns
>
> Regards, Steve Kelly
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of tony steinke
> Sent: Wednesday, June 19, 2002 6:12 PM
> To: [log in to unmask]
> Subject: Re: [TN] Immersion Tin
>
> Steve,
> If you do not prefer the SERA testing to measure/evaluate
> the amount of copper migration, what method/test are you doing to insure
> that you are giving your customer a good solderable surface. Please
> explain?
> Tony Steinke
> AIT-Atlanta Inc.
> ----- Original Message -----
> From: "Steve Kelly" <[log in to unmask]>
> To: <[log in to unmask]>
> Sent: Wednesday, June 19, 2002 11:13 AM
> Subject: Re: [TN] Immersion Tin
>
>
> > SERA will not help you - it is only a tool to measure tin /copper
> > concentrations . We have been running immersion tin for 5 years with
> no
> > issues but only one thermal excursion is allowed. The tin forms a
> > copper/tin intermetallic after thermal. We even silkscreen before tin
> to
> > eliminate this bake cycle. Regards Steve
> >
> > -----Original Message-----
> > From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan
> > Sent: Wednesday, June 19, 2002 12:07 PM
> > To: [log in to unmask]
> > Subject: Re: [TN] Immersion Tin
> >
> > Hi Tony,
> >
> > we experienced poor wave soldering after 2 reflows with immersion tin.
> > So,
> > please give me a few hints on SERA. Is it a test that the board house
> > will
> > do, or it has to be at our incoming? Does it imply additional charges?
> > Where
> > can I read more?
> >
> > Thanks,
> > Ioan
> >
> > > -----Original Message-----
> > > From: tony steinke [SMTP:[log in to unmask]]
> > > Sent: Wednesday, June 19, 2002 11:19 AM
> > > To:   [log in to unmask]
> > > Subject:      Re: [TN] Immersion Tin
> > >
> > > Grant,
> > > Having installed the Cookson(Dexter) FST  chemistry a couple of
> years
> > > ago at my previous employer, there are concerns that you should be
> > aware
> > > of.
> > > The immersion tin
> > > process is a beautiful thing if applied and processed properly. Some
> > of
> > > the
> > > major
> > > issues that I experienced were:
> > > Solder mask adhesion(you should tape test any incoming product)
> > > Request that SERA(sequential electromigration reduction analysis)
> test
> > be
> > > performed.
> > > And the biggest problem was getting acceptable solderability on
> second
> > > pass
> > > wave solder
> > > or second pass solder paste. The copper migration greatly
> accelerates
> > > during
> > > any thermal
> > > excursion, but that is what the SERA testing will show you.
> > > Tony Steinke
> > > [log in to unmask]
> > >
> > > ----- Original Message -----
> > > From: "Grant Emandien" <[log in to unmask]>
> > > To: <[log in to unmask]>
> > > Sent: Wednesday, June 19, 2002 3:06 AM
> > > Subject: [TN] Immersion Tin
> > >
> > >
> > > > Members,
> > > >
> > > > A PCB supplier has requested us to evaluate immersion tin as a
> > finish.
> > > > Immediate concerns raised were shelf life, solderability,
> whiskers,
> > etc.
> > > > Researching the archives has noted similar as well as opposing
> views
> > and
> > > > concerns. In addition to possible problems arising from immersion
> > tin
> > > > finish, what PCB fabricator process changes may contribute to
> > possible
> > > > reliability and solderability concerns and how this impacts
> > production
> > > > processes such as reflow. The proprietary chemistry used is
> MacStan
> > HSR
> > > from
> > > > Macdermid.
> > > >
> > > > Anyone willing to share experiences and guide me towards making an
> > > informed
> > > > decision.
> > > >
> > > > TIA
> > > > Grant
> > > >
> > > >
> > > >
> > **********************************************************************
> > > > Notice:
> > > >
> > > > This email transmission contains confidential information which is
> > the
> > > property of the sender. The information is intended only for the use
> > of
> > > the
> > > addressee. If you are not the intended recipient, you are hereby
> > notified
> > > that any disclosure, copying or distribution of the contents of this
> > > e-mail
> > > transmission, or the taking of any action in reliance thereon or
> > pursuant
> > > thereto, is strictly prohibited. Should you have received this email
> > in
> > > error, please immediately notify us by telephone to arrange for
> return
> > of
> > > the documentation comprising this transmission. In no event will
> > Tellumat
> > > (Pty) Ltd or the sender of this email be liable to any party for any
> > > direct,
> > > indirect, special or other consequential damages for any use of this
> > > email,
> > > or on any other hyper linked website, including, without limitation,
> > any
> > > lost profits, business interruption, loss of programs or other data
> on
> > > your
> > > information handling system or otherwise, even if we are expressly
> > advised
> > > of the possibility of!
> > > >  such damages.
> > > >
> > > >
> > **********************************************************************
> > > >
> > > >
> > >
> >
> ------------------------------------------------------------------------
> > --
> > > -------
> > > > Technet Mail List provided as a free service by IPC using LISTSERV
> > 1.8d
> > > > To unsubscribe, send a message to [log in to unmask] with following
> > text
> > > in
> > > > the BODY (NOT the subject field): SIGNOFF Technet
> > > > To temporarily halt delivery of Technet send e-mail to
> > [log in to unmask]:
> > > SET Technet NOMAIL
> > > > To receive ONE mailing per day of all the posts: send e-mail to
> > > [log in to unmask]: SET Technet Digest
> > > > Search the archives of previous posts at:
> > > http://listserv.ipc.org/archives
> > > > Please visit IPC web site http://www.ipc.org/html/forum.htm for
> > > additional
> > > > information, or contact Keach Sasamori at [log in to unmask] or
> > 847-509-9700
> > > ext.5315
> > > >
> > >
> >
> ------------------------------------------------------------------------
> > --
> > > -------
> > >
> > >
> >
> ------------------------------------------------------------------------
> > --
> > > -------
> > > Technet Mail List provided as a free service by IPC using LISTSERV
> > 1.8d
> > > To unsubscribe, send a message to [log in to unmask] with following
> text
> > in
> > > the BODY (NOT the subject field): SIGNOFF Technet
> > > To temporarily halt delivery of Technet send e-mail to
> > [log in to unmask]:
> > > SET Technet NOMAIL
> > > To receive ONE mailing per day of all the posts: send e-mail to
> > > [log in to unmask]: SET Technet Digest
> > > Search the archives of previous posts at:
> > http://listserv.ipc.org/archives
> > > Please visit IPC web site http://www.ipc.org/html/forum.htm for
> > additional
> > > information, or contact Keach Sasamori at [log in to unmask] or
> > 847-509-9700
> > > ext.5315
> > >
> >
> ------------------------------------------------------------------------
> > --
> > > -------
> >
> >
> ------------------------------------------------------------------------
> > ---------
> > Technet Mail List provided as a free service by IPC using LISTSERV
> 1.8d
> > To unsubscribe, send a message to [log in to unmask] with following text
> > in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt delivery of Technet send e-mail to
> [log in to unmask]:
> > SET Technet NOMAIL
> > To receive ONE mailing per day of all the posts: send e-mail to
> > [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at:
> > http://listserv.ipc.org/archives
> > Please visit IPC web site http://www.ipc.org/html/forum.htm for
> > additional
> > information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700
> > ext.5315
> >
> ------------------------------------------------------------------------
> > ---------
> >
> >
> ------------------------------------------------------------------------
> --
> -------
> > Technet Mail List provided as a free service by IPC using LISTSERV
> 1.8d
> > To unsubscribe, send a message to [log in to unmask] with following text
> in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt delivery of Technet send e-mail to
> [log in to unmask]:
> SET Technet NOMAIL
> > To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> > Please visit IPC web site http://www.ipc.org/html/forum.htm for
> additional
> > information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700
> ext.5315
> >
> ------------------------------------------------------------------------
> --
> -------
>
> ------------------------------------------------------------------------
> ---------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
> SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> ------------------------------------------------------------------------
> ---------
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
> SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2