TECHNET Archives

October 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 1 Oct 2004 11:49:57 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Reeves, Tim R." <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Reeves, Tim R." <[log in to unmask]>
Parts/Attachments:
text/plain (52 lines)
I have a datasheet that says Young's Modulus for N4000-13 is 4.2E6 psi (X)
and 3.3E6 psi (Y)
Of course those are "typical values" as it will depend on the glass style
involved.

Tim Reeves
Lamination Engineer
Tyco Electronics | Printed Circuit Group | Dallas Division
1270 Monmouth Cutoff Road, Dallas, OR 97338
503.623.1000 Ext.1120


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Werner Engelmaier
Sent: Thursday, September 30, 2004 9:15 AM
Subject: 2nd Nelco4000-13


 Hi 'Netters,

NELCO4000-13 dat sheet gives no modulus. Also it gives "Z Axis Expansion 
[50°C to 260°C] = 3.5%"--does this mean CTE (z) = 167 ppm/°C? [Sure is a
strange 
way to give a CTE]

Regards,
Werner Engelmaier

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2