I have a datasheet that says Young's Modulus for N4000-13 is 4.2E6 psi (X) and 3.3E6 psi (Y) Of course those are "typical values" as it will depend on the glass style involved. Tim Reeves Lamination Engineer Tyco Electronics | Printed Circuit Group | Dallas Division 1270 Monmouth Cutoff Road, Dallas, OR 97338 503.623.1000 Ext.1120 -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Werner Engelmaier Sent: Thursday, September 30, 2004 9:15 AM Subject: 2nd Nelco4000-13 Hi 'Netters, NELCO4000-13 dat sheet gives no modulus. Also it gives "Z Axis Expansion [50°C to 260°C] = 3.5%"--does this mean CTE (z) = 167 ppm/°C? [Sure is a strange way to give a CTE] Regards, Werner Engelmaier --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------