TECHNET Archives

January 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Sat, 9 Jan 1999 02:29:10 +0200
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Gabriela Bogdan <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
Gabriela Bogdan <[log in to unmask]>
Parts/Attachments:
text/plain (54 lines)
[log in to unmask] wrote:

> Gaby,
>
> Sorry about your troubles. I've never run into it with through hole
> devices, but many times with SMT
> types having been reflowed and often needing touched-up because of
> poor solder termination
> solderability.
>
> It sounds and looks (in x-section) like a smilar problem. The fine
> coil wires become detached under
> thermal stress because of dissimilar expansion rates at the attachment
> "legs."
>
> We solved some, not all, problems by changing a supplier once to
> improve solderability. In another
> instance, we more carefully watched our profiles to do everything
> possible to avoid touch-up.
>
> Good luck,
>
> Earl Moon
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################

 Thanks, Earl!
Gaby

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2