Hello Technet !
We intend to switch our PTH process from thin copper electroless plus
electrolytic strike to thick ( hot ) electroless , 2 microns thick . The
line will be loaded with baskets , so we do expect the PCBs will be
oxidized.We are considering some kind of chemical treatment prior to dry
film lamination instead of pumice scrub.Wjhat kind of treatment is recommended ?

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2