Not too familiar with Multicore naming convention these days, but RA
(instead RMA or R) in the name suggests you have an Activated Rosin instead
of a RMA or Madly activated Rosin. If this is the case you will need to
clean.
Regards
Mike Fenner
Applications Engineer, European Operations
Indium Corporation
T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Leadfree: www.Pb-Free.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Phillip Hinton
Sent: Thursday, September 19, 2002 3:39 PM
To: [log in to unmask]
Subject: Re: [TN] HMP Solder Paste
Pat
Multicore has been formulating fluxes for HMP solders for along time and I
understand this one is of the better ones. The solder paste is great for
use where a solder such as HMP is needed. If you are going to use it for
applications other than through hole soldering and you operating temperature
is 150oC or greater, I suggest you look at the long term aging problems with
high-lead solders. These high-lead solders tend to coarsen badly during
aging and develop large grains with weak grain boundaries which fracture
easily if placed in tension, shear is much better. Don't use for surface
mount if the operating temperatures approach even 125oC for a long periods.
( I have seen recently some microsections that were supposedly subjected to
only 125oC for about a week that showed large grains and cracking). I
would suggest you take your soldered samples and subject them to operating
temperature for about a 1000 hours and then test th! em mechanically.
Phil
Hinton ---------------------------------------------------------------------
------------ Technet Mail List provided as a free service by IPC using
LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with
following text in the BODY (NOT the subject field): SIGNOFF Technet To
temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315 -------------------------------------------------------------------
--------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|