TECHNET Archives

October 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 1 Oct 2009 20:21:41 +0000
Reply-To:
Subject:
Content-Transfer-Encoding:
base64
MIME-Version:
1.0
Content-Type:
text/plain
From:
Vladimir Igoshev <[log in to unmask]>
Parts/Attachments:
text/plain (1 lines)
And the reason for that is that Ni-P is amorphous, compared to a polycrystalline electrolytic Ni

Vladimir
------Original Message------
From: David D. Hillman
Sender: TechNet
To: [log in to unmask]
ReplyTo: TechNet E-Mail Forum
ReplyTo: [log in to unmask]
Sent: Oct 1, 2009 16:06
Subject: Re: [TN] Ductility of nickel

Hi Steve - I can't seem to put my fingers on the references but I believe 
that the elongation of High Phos Enickel is 1-1.5% and the elongation of 
electroplated nickel ranges from 10-30%. Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]




Steve Kelly <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
10/01/2009 02:43 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Steve Kelly <[log in to unmask]>


To
[log in to unmask]
cc

Subject
[TN] Ductility of nickel






Hi All,

What is the approximate difference in ductility between electroless nickel
(as used in an ENIG line - mid phos- 40 -80 micro inches in thickness) and
the same amount as electroplated to QQN-290. Thanks. Steve Kelly

 

Steve Kelly (PLEASE NOTE NEW E-MAIL ADDRESS)

(416) 750-8433 (work)

(416) 750-0016 (fax)

(416) 577-8433 (cell)

 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------




SENTEC

11 Canadian Road, Unit 7.

Scarborough, ON M1R 5G1

Tel: (416) 899-1882

Fax: (905) 882-8812

www.sentec.ca


ATOM RSS1 RSS2