TECHNET Archives

October 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Kelly <[log in to unmask]>
Date:
Thu, 1 Oct 2009 19:48:37 +0000
Reply-To:
Subject:
Content-Transfer-Encoding:
base64
MIME-Version:
1.0
Content-Type:
text/plain
From:
Vladimir Igoshev <[log in to unmask]>
Parts/Attachments:
text/plain (1 lines)
Electroless is more brittle, as it's in fact an Ni-P alloy.



Vladimir

------Original Message------

From: Steve Kelly

Sender: TechNet

To: [log in to unmask]

ReplyTo: TechNet E-Mail Forum

ReplyTo: Steve Kelly

Sent: Oct 1, 2009 15:43

Subject: [TN] Ductility of nickel



Hi All,



What is the approximate difference in ductility between electroless nickel

(as used in an ENIG line - mid phos- 40 -80 micro inches in thickness) and

the same amount as electroplated to QQN-290. Thanks. Steve Kelly



 



Steve Kelly (PLEASE NOTE NEW E-MAIL ADDRESS)



(416) 750-8433 (work)



(416) 750-0016 (fax)



(416) 577-8433 (cell)



 





---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------







SENTEC

11 Canadian Road, Unit 7.

Scarborough, ON M1R 5G1

Tel: (416) 899-1882

Fax: (905) 882-8812

www.sentec.ca


ATOM RSS1 RSS2