I last visited Electroply in 2005 to qualify them as a supplier for black
FR4. You're right, their phone is disconnected, their website is down, and
their email address doesn't work. They were the last supplier I could find
that had the black FR4. In 2005 they were partnering with an overseas
company on some laminate material, perhaps they got bought out? I know who
their main customer for the black (and blue) FR4 was, I'll try to see who
they are buying from now.
Tom
Ralph Richart <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
10/01/2009 02:24 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Ralph Richart <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] Black Laminate
Once upon a time we purchased black FR4 laminate from Electroply.
Electroply seems to be out of business - their website does not work and
the phones are disconnected.
The question: Does anyone know of a source for black FR4 these days?
Thanks for the help...
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|