I saw a presentation on this material at an IMAPS meeting. It is based on
German engineering using Molybdenum powder in a mixture to meet specified
TCE and thermal attributes. It was interesting, expensive, an would demand
some thoughtful design work.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Randy Bock Sr.
Sent: Thursday, May 31, 2007 8:03 AM
To: [log in to unmask]
Subject: Re: [TN] Conductive Cooling thru Pre-Prig material
We do not use this type of material but did find the web link very
interesting...
Randy Bock Sr.
Quality Engineer
Enterprise Quality Assurance
AddressRight Printers
(email) [log in to unmask]
Newtown Building 2
203 270-4931 Ext
8-426-4931 In
203 270-4982 Fax
This e-mail message may contain confidential, proprietary and/or privileged
information. It is intended only for the use of the intended recipient(s).
If you receive this in error, please immediately advise the sender by reply
e-mail and delete this e-mail message. Any disclosure, copying,
distribution or use of the information contained in the e-mail to or by
anyone other than the intended recipient is strictly prohibited. Any views
expressed in this message are those of the individual sender, except when
the sender specifically states them to be the views of the company.
Thank You.
Steve Gregory <[log in to unmask]> Sent by: TechNet
<[log in to unmask]>
05/31/2007 07:57 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to Steve Gregory
<[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [TN] Conductive Cooling thru Pre-Prig material
Good Morning Terry!
Although I don't have any experience with this material, it looks very,
very interesting. Check this out:
http://www.stablcor.com/presentation/
At the last company I worked at we were about to try the material in a
single board computer assembly that we had the task of ruggedizing, but
we ran into some issues with our customer that I won't get into...
Only drawback that I can initially see is that it is electrically
conductive and only licensed to a half-dozen fabs shops here in the US.
Maybe there might be some way that you can use this in your design.
Steve Gregory
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Terry Kozlyk
Sent: Thursday, May 31, 2007 6:02 AM
To: [log in to unmask]
Subject: [TN] Conductive Cooling thru Pre-Prig material
Technetters;
I have a 6 layer PCB with about 8 HOT DPAK components. The tabs are
electrically hot so I cannot just draw the heat directly thru a copper
fill brought out to the edge of the PCB.
I need electrical isolation, BUT high thermal conductivity between 2
adjacent layers.
Can anyone recommend what material they have specified to be used for
pre-prig that conducted the heat to the adjacent layer?
Voltage max is about 50 volts so I could probably go down to 2 or 3 mil
pre-prig.
Nothing special about this PCB; about 5" x 5".
The fab houses I solicited for info still haven't replied so I am
curious.
Any leads, products or websites would be appreciated.
Regards
TDK
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|