That was nicely and concisely summarized George.
Best regards,
Joe
In a message dated 11/24/2006 7:51:25 A.M. Pacific Standard Time,
[log in to unmask] writes:
You've stated correctly the dilemma companies are facing. You've
comment/question about option 2 creating a reliability concern and also
invalidating the manufacturers warranty is also correct. Companies are
going to have to make their own risk assessments. Unfortunately, many
of those decisions are not knowledge based decisions because there isn't
good documented information available. The recommendations I've made
internally are:
1. Use SnPb assembly whenever possible
2. Use Pb-Free components and processes when product needs to be RoHS
6/6 compliant.
3. When forced into mixed alloy assembly:
a. For RoHS 6/6 product, use Pb-Free processes (245-260C) when
all components are compatible with Pb-Free processes.
b). For RoHS 5/6 product, use maximum SnPb process temperatures
(225- 235C) whenever there are components not compatible with
Pb-Free processes (i.e., don't exceed the maximum
temperature the MSL was tested at by the component vendor.
c). Do not re-ball Pb-Free area array packages with SnPb balls.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|