I'll second what Doug stated as I have used a batch system with 18% Kyzen A4520 at 120°C that successfully removes "no clean" residues from assemblies that have been sitting for up to 2 weeks. One thing to remember is that not all no-cleans are synonymous with low residue. Some "no clean" residues will look 10X worse after being exposed to a cleaning process. I suggest contacting your solder/flux supplier and ask what they recommend.
Good Luck
Steve
Steve Sauer, CEPM
Sr. Project Engineer
Northrop Grumman Xetron
Cincinnati, OH
513-881-3368
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas O. Pauls
Sent: Wednesday, March 05, 2008 9:00 AM
To: [log in to unmask]
Subject: Re: [TN] Cleaning No-clean
Dan,
Yes, many of the low residue fluxes can be successfully cleaned with the right saponifier and batch wash parameters. I would suggest that you contact Kyzen Corporation. They have done a great deal of work on chemistries to clean low residue fluxes, in both in-line and batch operations. They have looked at almost every flux made. We are a Kyzen house here at Rockwell. They support their products very well.
Charlie Pitarys of Kyzen regularly hangs out on this forum. I suspect he will be contacting you.
Doug Pauls
Rockwell Collins
Dan Mauro <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
03/05/2008 06:35 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to Dan Mauro <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] Cleaning No-clean
Folks,
I have a need to clean No-clean residue from PCBA's. Can this be
achieved with water washer and some type of saponifier ? Can anybody
suggest a batch process?
Thanks,
Dan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|