"John Sater" <[log in to unmask]> Wrote:
|
| Hello Techneters
|
| I wonder what are the advantages of DSTF which make this
| type of
| copper finish gaining so much popularity?
|
| Thanks,
|
| JS
|
John, the theoretical advantages are increased adhesion of dry film to the
plated topography which is usually the side applied to the B stage to make
laminate, lower profile for etch at the copper-laminate interface, and
possibly reduced cleaning costs. Polyclad, Nelco, AlliedSignal, etc. can
provide technical literature discussing DSTF or RTF. It is not necessarily a
drop in product. Precleaning is different, lamination can be different, hold
times, rework, and possibly oxide are processes that need to be optimized.
Jana Carraway
Maxtek -- the Maxim/Tektronix Multichip Module facility
tel 503.627.2063, fax 503.627.4651
email [log in to unmask], www.maxtek.com
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|