Hi Jim!
There are a lot of coatings that have a UV tracer added to it so that it
glows under a UV light and makes it very easy to inspect. At the last
place I worked we had a UV light in the spray booth where the coating
was done, and the operator could easily see where he needed to spray as
he was doing the coating.
-Steve Gregory-
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of West, Jim
Sent: Thursday, October 19, 2006 8:29 AM
To: [log in to unmask]
Subject: [TN] Colored conformal coating
Does anyone know of any conformal coating that has a color to it instead
of clear? We are currently spraying some conformal coating manually,
and with it being clear, it is not always guaranteed that the operator
hits all required areas.
Thanks,
Jim West
Engineering Manager
Nexergy Inc.
www.nexergy.com
tel: (614) 351-6216
fax: (614) 324-1979
This email message and all attachments transmitted with it are intended
solely for the use of the addressee(s) and may contain legally
privileged, protected or confidential information. If you believe that
you have received this message in error, please notify the sender
immediately by email reply and please delete this message from your
computer and destroy any copies.
--------------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|