Hi Jim! There are a lot of coatings that have a UV tracer added to it so that it glows under a UV light and makes it very easy to inspect. At the last place I worked we had a UV light in the spray booth where the coating was done, and the operator could easily see where he needed to spray as he was doing the coating. -Steve Gregory- -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of West, Jim Sent: Thursday, October 19, 2006 8:29 AM To: [log in to unmask] Subject: [TN] Colored conformal coating Does anyone know of any conformal coating that has a color to it instead of clear? We are currently spraying some conformal coating manually, and with it being clear, it is not always guaranteed that the operator hits all required areas. Thanks, Jim West Engineering Manager Nexergy Inc. www.nexergy.com tel: (614) 351-6216 fax: (614) 324-1979 This email message and all attachments transmitted with it are intended solely for the use of the addressee(s) and may contain legally privileged, protected or confidential information. If you believe that you have received this message in error, please notify the sender immediately by email reply and please delete this message from your computer and destroy any copies. -------------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------