TECHNET Archives

March 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
"Tempea, Ioan" <[log in to unmask]>
Date:
Mon, 29 Mar 2004 09:43:31 -0500
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Tempea, Ioan" <[log in to unmask]>
Parts/Attachments:
text/plain (52 lines)
Thanks Steve,

I assume this applies to the collapsed height, like spheres with a diameter
of 0.050" will be 0.0375" high after soldering. But is it possible to put
some tolerances on this, let's say <the height after soldering will be
0.037" +/- 0.004"> ? Of course, it is assumed that the process is stable,
consistent volume of printed paste, and consistent reflow recipe.

Best regards,
Ioan

> -----Original Message-----
> From: [log in to unmask] [SMTP:[log in to unmask]]
> Sent: Monday, March 29, 2004 9:09 AM
> To:   [log in to unmask]; [log in to unmask]
> Subject:      Re: [TN] BGA height after soldering
>
> Hi Ioan!
>
> A good figure to use is 25%...of course this goes without saying the
> figure only applies to eutectic balls.
>
> -Steve Gregory-
>
>
>
>
>       Hi Techos,
>
>       a question about BGA collapsing. I have an application where we have
> to fit
>       an assembled PCB into a tight place. The highest part is a BGA and I
> wonder
>       if anybody has knowledge of the height tolerances after soldering.
>
>       Thenks,
>       Ioan
>
>
>
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2