The correct patent numbers to reference are 4312692 and 4314870. Both
patents refer to the mechanical mounting of surface mount components using a
cured adhesive.
We are in the process of setting up a small assembly shop and would be
interested in the effects of the assertion of these patents.
Jeffrey A. McGlaughlin
PWB Designer
Battelle Memorial Institute
Columbus Ohio
-----Original Message-----
From: Matthias Mansfeld [SMTP:[log in to unmask]]
On 14 Apr 98 at 19:21, SteveZeva wrote:
....
> found the following post:
> >Posted by Mike C on April 14, 1998 at 18:01:28:
.....
> >USP 4,812,692 USP 4,814,870
>
> Is this something that we should really worry about? Anybody know?
I tried to find these patents on the IBM Patent Server, but I found
only non-SMT topics under these numbers.
USP 4,812,692
http://www.patents.ibm.com/details?patent_number=4812692:
"Motor" (Mitsubishi)
USP 4,814,870
http://www.patents.ibm.com/details?patent_number=4814870:
"Portable infrared imaging apparatus" (Comprix)
None is from Matsushita, none is about SMT. I asked Mike C in the
smtnet.com forum to provide more informations about these patents.
Perhaps IPC could put the letter Mike C and Steve Gregory mentioned
in this and/or the DesignerCouncil?
-----------------------------------------------
Matthias Mansfeld Elektronik
* Leiterplattenlayout, Bestueckung
Am Langhoelzl 11, D-85540 Haar
Postfach 1143, D-85529 Haar
Tel.: 089/4620 0937, Fax: 089/4620 0938
E-Mail: [log in to unmask]
Internet: http://home.t-online.de/home/matthias.mansfeld
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|