TECHNET Archives

May 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Paul Klasek <[log in to unmask]>
Reply To:
"TechNet E-Mail Forum." <[log in to unmask]>, Paul Klasek" <[log in to unmask]>
Date:
Mon, 24 May 1999 10:27:27 +1000
Content-Type:
text/plain
Parts/Attachments:
text/plain (70 lines)
While we're on the 20 mil subject ;
the same apply on the polyimide ? ; as they have better release ratio than
SS ?
Any comments on plastic stencils in general ?

Thanks        paul

-----Original Message-----
From: Stephen R. Gregory [mailto:[log in to unmask]]
Sent: Saturday, 15 May 1999 2:04
To: [log in to unmask]
Subject: Re: [TN] Stencil Thickness


In a message dated 5/14/99 8:59:39 AM Pacific Daylight Time,
[log in to unmask] writes:

<< Hi Technetters,

 What kind of stencil thickness you would recommend for 20 mil pitch QFP?

 4, 5 or 6 mil ?

 Thanks in advance.
 Poh >>

 Hi Poh!

I always get a 6-mil with the industry standard aperture reduction (20%
smaller)... always  works for me without a problem.

-Steve Gregory-

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2