From what you're saying I would try a fresh paste container as received and
see what happens. WS pastes can be effected by moisture take up, but a new
jar fresh from the supplier should be OK to start. If the incidence is
unchanged then you will have at least eliminated this from your
investigations. Water take up by the paste will result in it steaming and
spattering the solder into small beads around each joint area. If it is
moisture uptake into the paste and you continue to use it then you can run
into other problems as the water content becomes more significant.
We have a short leaflet in which the issue of Solder balls/beads is defined
and addressed. If you would like a copy let me know off net.
Best regards
Mike Fenner
Applications Engineer, European Operations
Indium Corporation
T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Leadfree: http://Pb-Free.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Jorge Rodriguez
Sent: Tuesday, August 21, 2001 7:57 PM
To: [log in to unmask]
Subject: [TN] Solder Beads (not solder balls)
Fellow technetters,
We are having tons of issues with solder beading, even on boards were we
didn't have the issue before. We're clueless, we suspect of the solder paste
(63-37 Water Soluble), it looks slumpy amd watery, but we're not sure. I
know solder beading can be solved by designing the stencils with home-base
aperture, but what we're seeing here is across the board, not just one
particular assembly but several. Does anyone have experience dealing with an
issue like this?, could solder beading caused by the oven profile or is it
more like solder paste related?
Any comments would be appreciated.
Jorge Rodriguez
Process Engineer
Varian Electronics Manufacturing
E-mail: [log in to unmask]
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|